Аннотации:
© Published under licence by IOP Publishing Ltd. The kinetics and reasons for metallic pipe wear of hot chamberzinc alloy die casting machines are established.Increasing metallic pipe wear components wear resistance is being achieved by means of die steel - 22 with electroslag remelting modification and electron-beamremelting modification and after the processes of nitriding and boriding besides.