A thermal study on peat oxidation behavior in the presence of an iron-based catalyst

Show simple item record

dc.contributor.author Khelkhal M.A.
dc.contributor.author Lapuk S.E.
dc.contributor.author Ignashev N.E.
dc.contributor.author Eskin A.A.
dc.contributor.author Glyavin M.Y.
dc.contributor.author Peskov N.Y.
dc.contributor.author Krapivnitskaia T.O.
dc.contributor.author Vakhin A.V.
dc.date.accessioned 2022-02-09T20:43:36Z
dc.date.available 2022-02-09T20:43:36Z
dc.date.issued 2021
dc.identifier.uri https://dspace.kpfu.ru/xmlui/handle/net/169847
dc.description.abstract Peat is a resource used for heat and energy, particularly in countries where peat is abundant and conventional fuels are not available. Some countries have made extensive use of peat resources to produce electricity and heat in addition to light hydrocarbons. By doing so, they were able to reduce the cost of importing fossil fuels. To the best of our knowledge, there is a lack of a detailed description of the peat oxidation process in the presence of other substances. Herein, the process of peat oxidation was studied in-depth by means of thermal analysis in the presence of iron tallate acting as a catalytic agent. Differential scanning calorimetry and thermogravimetric analysis demonstrated an oil-like oxidation behavior during the combustion of the used peat. The process of peat oxidation includes two main regions: low-temperature oxidation (LTO), which occurs during the oxidation of light hydrocarbons, followed by the so-called high-temperature oxidation (HTO), which includes the oxidation of the obtained coke-like product. Moreover, the application of non-isothermal kinetics experiments based on the isoconversional and model approach principle have confirmed the role of 2% iron tallate in peat mass by improving the oxidation rate at low-and high-temperature oxidation (HTO) regions. The results obtained from this study have proven that the added catalyst improves efficiency with regards to the energy activation in the process by leading to its significant decrease from 110.8 ± 7.8 kJ/mol to 81.8 ± 7.5 kJ/mol for LTO and from 157.8 ± 19.1 kJ/mol to 137.6 ± 9.3 kJ/mol for HTO. These findings clearly confirm the improvement in the rate of the process by shifting the LTO and HTO peaks to lower regions in the presence of the catalyst. These results further emphasize the possible impact which could be generated by the application of thermally enhanced oil recovery methods on peat development and exploitation.
dc.subject Catalysts
dc.subject DSC
dc.subject Iron oxide nanoparticles
dc.subject Non-isothermal kinetics
dc.subject Oxidation
dc.subject Peat
dc.subject TG
dc.subject Thermal analysis
dc.subject Unconventional resources
dc.title A thermal study on peat oxidation behavior in the presence of an iron-based catalyst
dc.type Article
dc.relation.ispartofseries-issue 11
dc.relation.ispartofseries-volume 11
dc.collection Публикации сотрудников КФУ
dc.source.id SCOPUS-2021-11-11-SID85118715579


Files in this item

This item appears in the following Collection(s)

  • Публикации сотрудников КФУ Scopus [24551]
    Коллекция содержит публикации сотрудников Казанского федерального (до 2010 года Казанского государственного) университета, проиндексированные в БД Scopus, начиная с 1970г.

Show simple item record

Search DSpace


Advanced Search

Browse

My Account

Statistics