dc.description.abstract | © 2017, Springer-Verlag GmbH Austria, part of Springer Nature. The Sc2SiO5single crystals doped with 0.001 at.% of the143Nd3+ion were studied by continuous-wave and pulse electron paramagnetic resonance methods. The g-tensors and hyperfine structure tensors for two magnetically non-equivalent Nd ions were obtained. The spin–spin and spin–lattice relaxation times were measured at 9.82 GHz in the temperature range from 4 to 10 K. It was established that three relaxation processes contribute to the spin–lattice relaxation processes. There are one-phonon spin–phonon interaction, two-phonon Raman interaction and two-phonon Orbach–Aminov relaxation processes. It was established that spin–spin relaxation time is of the same magnitude for neodymium ion doped in Sc2SiO5and in Y2SiO5. | |
dc.relation.ispartofseries | Applied Magnetic Resonance | |
dc.title | EPR Study of Sc<inf>2</inf>SiO<inf>5</inf>:Nd<sup>143</sup>Isotopically Pure Impurity Crystals | |
dc.type | Article | |
dc.relation.ispartofseries-issue | 1 | |
dc.relation.ispartofseries-volume | 49 | |
dc.collection | Публикации сотрудников КФУ | |
dc.relation.startpage | 53 | |
dc.source.id | SCOPUS09379347-2018-49-1-SID85033485899 |