Flocculating capability reducing the water solutions of polyethylene oxide (PEO) during storage

Show simple item record

dc.contributor.author Kuz'min A.
dc.contributor.author Mazitova V.
dc.contributor.author Onishchenko A.
dc.contributor.author Arkhipov V.
dc.contributor.author Kostochko A.
dc.date.accessioned 2018-09-17T20:32:51Z
dc.date.available 2018-09-17T20:32:51Z
dc.date.issued 1995
dc.identifier.issn 0204-3556
dc.identifier.uri https://dspace.kpfu.ru/xmlui/handle/net/133653
dc.description.abstract The changes of hydrodynamic characteristics and macromolecule dimensions of 0.2% water solution PEO are investigated depending on duration of the isothermal endurance. By the methods of viscosimetry, NMR and molecular-mass distribution it is ascertained that in the first 20-28 days of solution endurance the decrease of flocculating capability of PEO is caused by the change of polymer chains conformation, and during further storage - by the chains destruction.
dc.relation.ispartofseries Khimiya i Tekhnologiya Vody
dc.title Flocculating capability reducing the water solutions of polyethylene oxide (PEO) during storage
dc.type Article
dc.relation.ispartofseries-issue 2
dc.relation.ispartofseries-volume 17
dc.collection Публикации сотрудников КФУ
dc.relation.startpage 125
dc.source.id SCOPUS02043556-1995-17-2-SID0029259387


Files in this item

This item appears in the following Collection(s)

  • Публикации сотрудников КФУ Scopus [24551]
    Коллекция содержит публикации сотрудников Казанского федерального (до 2010 года Казанского государственного) университета, проиндексированные в БД Scopus, начиная с 1970г.

Show simple item record

Search DSpace


Advanced Search

Browse

My Account

Statistics